自动喷粉线上六轴机械臂,老板常以为“手稳了,膜厚就稳”。真跑起来才发现:工件内角漏底、平面橘皮、换色一拖半小时,问题多半不在机器人本身,而在前处理、粉末流化、静电匹配这三段没对齐。
The automatic powder spraying line has a six axis robotic arm, and the boss often thinks that 'once the hand is stable, the film thickness will be stable'. It was only after running that I realized that the problems with the leaking bottom of the inner corner of the workpiece, flat orange peel, and color change that took half an hour were mostly not related to the robot itself, but rather to the misalignment of pre-processing, powder fluidization, and electrostatic matching.
先看前处理。喷粉不像喷漆能靠“盖一层”遮丑,磷化或硅烷膜没做透,油污残留,粉末烤完一掰就掉。机器人喷得再准,附着力也是零。前处理槽液温度、游离酸度、水洗电导率,每天记一笔,比事后补喷划算得多。
Let's first look at the pre-processing. Spraying powder is not like painting, which can rely on "covering a layer" to cover up ugliness. The phosphating or silane film is not fully penetrated, leaving oil stains, and the powder will fall off as soon as it is baked. Even if the robot sprays accurately, its adhesion is zero. Recording the temperature, free acidity, and washing conductivity of the pre-treatment tank solution once a day is much more cost-effective than re spraying afterwards.

再看粉末状态。流化桶气压偏小,粉末结块、吐粉一顿一顿;气压偏大,粉云飘散,回收系统吃不下,内角反而进不去。流化板该换就换,别等吐粉断续了才想起。回收旋风和滤芯压差每周看一次,压差爬升快,说明细粉积压,膜厚马上飘。
Check the powder state again. The air pressure in the fluidized bed drum is too low, causing powder to clump and spit out one after another; The air pressure is too high, causing the powder cloud to scatter and the recycling system to be unable to take it in. As a result, the interior angle cannot enter. If the fluidized bed needs to be replaced, replace it. Don't wait until the powder discharge is intermittent before thinking about it. Check the pressure difference between the recycling cyclone and the filter element once a week. If the pressure difference rises quickly, it indicates that the fine powder is accumulating and the film thickness is about to float.
第三是静电参数。机器人手腕带的是喷杯还是喷笔、电压给多少、雾化气压多大,得按工件形状分档。平面件电压可稍高、出粉量大;深腔、内角要降压、减气、多道薄喷,靠“法拉第笼”硬冲只会越喷越漏。程序里别只存一条轨迹,按大面—棱边—内腔分三段参数,膜厚才压得平。
The third is electrostatic parameters. Whether the robot wrist strap is a spray cup or a spray pen, how much voltage is applied, and how much atomization pressure is applied, need to be classified according to the shape of the workpiece. The voltage of flat parts can be slightly higher and the powder output can be large; Deep cavities and inner corners require pressure reduction, gas reduction, and multiple thin sprays. Relying on a "Faraday cage" for hard flushing will only result in more and more leaks. Don't just store one trajectory in the program, divide it into three parameters: large surface, edge, and inner cavity, in order to flatten the film thickness.
换色是隐形节拍杀手。同色连喷没事,一换深浅色,管路、喷杯、回收粉都得清。别信“吹两分钟就干净”,浅色接深色还好,深色转浅色,残粉一混就是麻点。真要提速,上双喷房轮换,或备两套喷杯管路,比逼着机器人干等强。
Changing colors is an invisible rhythm killer. Same color continuous spraying is fine. When changing between light and dark colors, the pipeline, spray cup, and recycled powder all need to be cleaned. Don't believe that 'blowing it for two minutes will clean it up'. It's okay to mix light colors with dark colors, but when dark colors turn into light colors, the residual powder will become pockmarks. If you really want to speed up, rotating between dual spray rooms or preparing two sets of spray cup pipelines is better than forcing robots to do it.
固化段也别脱节。粉末标称180℃/15min是工件实测温度,不是炉表温度。厚板吸热慢,芯部没到温,交联不够,百格一刀就掉。炉温测试仪每季度插一次工件最厚处,比天天盯仪表有用。
Don't disconnect the solidification section either. The nominal temperature of the powder at 180 ℃/15min is the measured temperature of the workpiece, not the furnace temperature. Thick plates absorb heat slowly, the core is not warm enough, the cross-linking is not enough, and it falls off with just one hundred cuts. The furnace temperature tester is inserted into the thickest part of the workpiece once every quarter, which is more useful than staring at the instrument every day.
机器人自动喷粉线省的是人工,不是省调试。前处理干净、粉末流得顺、静电分档、换色有预案、炉温按工件校——这五样盯住,膜厚才真稳,返工才真降。
The robot automatic powder spraying line saves labor, not debugging. Clean pre-treatment, smooth powder flow, electrostatic classification, color change plan, and furnace temperature calibration according to the workpiece - these five measures are closely monitored to ensure stable film thickness and reduced rework.
本文由机器人自动喷粉线友情奉献。更多有关的知识请点击:http://www.sdcjtz.com 我们将会对您提出的疑问进行详细的解答,欢迎您登录网站留言.
This article is a friendly contribution from the robot automatic powder spraying line. For more information, please click: http://www.sdcjtz.com We will provide detailed answers to your questions. You are welcome to log in to our website and leave a message
扫码添加微信了解更多